Customization: | Available |
---|---|
Material: | Zirconia-Corundum, Zro2 |
Refractoriness (℃): | 1580< Refractoriness< 1770, 1580< Refractoriness< 1770 |
Still deciding? Get samples of US$ 2000/Ton
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Fused Cast AZS block as an important role used in Glass Furnace is made of pure alumina powder and zircon sand and is composed of three main chemical components of Al2O3, ZrO2 and SiO2,most widely used materials both in glass contact and superstructure of glass melting furnaces. The products are made of high pure material, fired at high temperature by advanced technology, with the advantages of high strength, high compression resistance, good thermal shock resistance, good performance in high temperature, good thermal conductivity,excelerosion resistance and used for linings of furnace in glass industries.
Features
Applications
Specifications
Physical And Chemical Indicators
Brand Properties |
AZS-41 | AZS-36 | AZS-33 | |
Chemical Analysis(%) | ZrO2 | 40 | 35 | 32 |
SiO2 | 13.0 | 14 | 15.5 | |
Na2O | 1.3 | 1.4 | 1.5 | |
Fe2O3 | 0.10 | 0.10 | 0.10 | |
TiO2 | 0.05 | 0.05 | 0.05 | |
Cold Crushing Strength (MPa) | 350 | 350 | 350 | |
Bulk Density (g/cm3) | Regular cast | 3.55 | 3.45 | 3.4 |
Void free | 4.00 | 3.78 | 3.70 | |
Apparent Porosity (%) | 1.3 | 1.5 | 2.0 | |
Refractoriness Under Load(ºC)@0.2MPa | 1700 | 1700 | 1700 | |
Thermal Linear Expansion(%)@1000ºC | 0.80 | 0.80 | 0.80 |